Incoloy 800 Plate Description
The chemical composition of Incoloy 800 alloy consists mainly of nickel, chromium and iron. Among them, nickel is the main element that improves the corrosion resistance of the alloy, chromium helps enhance the oxidation resistance and high-temperature strength of the alloy, and iron provides the matrix structure of the alloy. In addition, the alloy also contains certain amounts of elements such as carbon, silicon and manganese to further enhance its overall performance. Incoloy 800 alloy has very good corrosion resistance, especially in reducing and oxidizing media. It also has good resistance to chemicals such as sulfuric acid, hydrochloric acid and alkaline solutions in high temperature environments. Incoloy 800 plate has good oxidation resistance in high temperature environments and can work at temperatures up to 1100°C for a long time. Lastly, Incoloy 800 plate has high yield strength and creep strength and can maintain its mechanical properties in high and low temperature environments.
Product Parameters
Product Name | Incoloy 800 Plate |
Thickness | 0.3mm-200mm |
Length | 2000mm, 2438mm, 3000mm, 5800mm, 6000mm, 12000mm, etc. |
Width | 40mm-600mm, 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc. |
Standard | ASTM, AISI, JIS, GB, DIN, EN, etc. |
Surface | BA, 2B, NO.1, NO.4, 4K, HL, 8K, etc. |
Certificate | ISO, SGS, BV |
Production Technology | Hot Rolling, Cold Rolling |
Chemical Composition
C | Al | Si | S | Ti | Cr | Mn | Fe | Ni | Cu |
0.1 max | 0.15 – 0.60 | 1.0 max | 0.015 max | 0.15 – 0.60 | 19.0 – 23.0 | 1.5 max | 39.5 min | 30.0 – 35.0 | 0.75 max |
Mechanical Properties
Tensile Strength (ksi) | 0.2% Yield Strength (ksi) | Elongation% in 2 inches |
75 | 30 | 30 |
Physical Performance
Units | Temperature in°C | |
Density | 7.94 g/cm³ | Room |
Specific Heat | 0.11 Kcal/kg.C | 21° |
Melting Range | 1357-1385°C | – |
Modulus of Elasticity | 196.5 KN/mm² | 20° |
Electrical Resistivity | 98.9 µΩ.cm | 20° |
Coefficient of Expansion | 14.4 µm/m °C | 20 – 100° |
Thermal Conductivity | 11.5 w/m-° K | 20° |
Scope of Application
The most common applications are heat treatment equipment, petrochemical pyrolysis piping systems, electric heating unit jackets and food processing equipment.
Related products
Inconel 601 Pipe
- OriginChina
- Delivery Time≥7 days
Inconel 718 Plate is a high-strength, heat-resistant alloy, ideal for high-temperature applications, offering excellent durability and corrosion resistance.
A36/Q235/S235JR Carbon Steel Coil
- OriginChina
- Delivery Time≥7 days
A36 carbon steel coil is a versatile, low-carbon steel with excellent weldability, machinability, and strength, widely used in construction, manufacturing, and structural applications for its durability and cost-effectiveness.
Carbon Steel Wire
- OriginChina
- Delivery Time≥7 days
Carbon steel wire is a durable, versatile material used in construction, manufacturing, and industrial applications for strength and flexibility.
1023 Cold Rolled Steel Coil
- OriginChina
- Delivery Time≥7 days
1023 cold rolled steel coil, offering excellent formability, strength, and surface quality. Ideal for automotive, industrial, and manufacturing applications requiring precision and durability.
loading…
已经是到最后一篇内容了!